Manufacturing / Gate treatment Pt. 2

Manufacturing / Gate treatment Pt. 2

Before

It is likely seen a serious sink mark at the confluence point of large cylinder moulding, if we employ side gate.

The sink mark appearance leads distortion and poor mechanical property, lower roundness.

After

Employing film or flash gate to eliminate weld line and improve the roundness tolerance.